Mayina Wamba Amalonda: Hastelloy X,UNS N06002, GH3536, W.Nr.2.4665

Hastelloy X ndi mtundu wa nickel base superalloy wokhala ndi chitsulo chambiri, chomwe chimalimbikitsidwa makamaka ndi yankho lolimba la chromium ndi molybdenum.Ili ndi anti-metallization ndi dzimbiri magwiridwe antchito, kupirira kwapakatikati ndi mphamvu zokwawa pansi pa 900 ℃, kuzizira komanso kutentha kwabwino komanso kuwotcherera.
Amagwiritsidwa ntchito popanga mbali za chipinda choyaka moto cha aero-injini ndi zigawo zina za kutentha kwambiri, pansi pa 900 ℃ kwa nthawi yayitali, kutentha kwanthawi yayitali mpaka 1080 ℃.

Hastelloy X Chemical Composition

Aloyi C Cr Ni Fe Mo W Al B Co Si Mn P S
Hastelloy X 0.05-0.15 20.5-23.5 bwino 17.0-20.0 8.0-10.0 0.2-1.0 ≤0.1 ≤0.005 0.5-2.5 ≤1.0 ≤1.0 ≤0.015 ≤0.01

Hastelloy X Physical Properties

Kuchulukana 8.3g/cm³
Malo osungunuka 1260-1355 ℃

Hastelloy X Mechanical Properties

Mkhalidwe Kulimba kwamakokedwe
Rm N/mm²
Zokolola mphamvu
Rp 0. 2N/mm²
Elongation
Monga%
Brinell kuuma
HB
Yankho mankhwala 690 275 30 > 241

 

Miyezo ya Hastelloy X ndi Mafotokozedwe

Chipinda / ndodo Waya Mzere / Coil Mapepala/Mbale Pipe/Tube Kupanga
Chithunzi cha ASTM B572ASME SB572AMS 5754 Mtengo wa AMS5798 Chithunzi cha ASTM B435ASME SB435AMS 5536 ASTM B662, ASME SB662
ASTM B619,ASME SB619
ASTM B626 ,ASME SB626AMS 5587
Mtengo wa AMS5754

Hastelloy X Zomwe Zilipo mu Sekonic Metals

Inconel 718 bar, inconel 625 bar

Hastelloy X Bars & Ndodo

Round mipiringidzo / Flat mipiringidzo / Hex mipiringidzo, Kukula Kuyambira 8.0mm-320mm, Amagwiritsidwa ntchito mabawuti, fastners ndi zina zopuma

waya wowotcherera ndi waya wamasika

Hastelloy X Waya

Perekani mu waya wowotcherera ndi waya wamasika mu mawonekedwe a koyilo ndikudula kutalika.

Mapepala & Plate

Hastelloy X pepala & mbale

M'lifupi mpaka 1500mm ndi kutalika mpaka 6000mm, Makulidwe kuchokera 0.1mm mpaka 100mm.

Hastelloy X yopanda msoko & chitoliro chowotcherera

Miyezo kukula ndi makonda gawo akhoza kupangidwa ndi ife ndi kulolerana yaing'ono

inconel strip, invar stirp, kovar chipwirikiti

Chithunzi cha Hastelloy X& kolala

Chikhalidwe chofewa komanso cholimba chokhala ndi AB chowala pamwamba, m'lifupi mpaka 1000mm

Fasterner & Other Fitting

Hastelloy X Fasteners

Zida za Hastelloy X mumitundu ya Bolts, zopangira, ma flanges ndi othamanga ena, malinga ndi kasitomala.

Chifukwa chiyani Hastelloy X?

1. Zabwino kwambiri makutidwe ndi okosijeni kukana pa kutentha kwambiri (> 1200 ℃)).
2. Mphamvu yabwino yotentha kwambiri.
3. Good formability ndi weldability.
4. Good kukana kupsinjika dzimbiri akulimbana.

Ntchito ya Hastelloy X:

Chifukwa cha kukana kwake kwa dzimbiri m'malo osiyanasiyana otentha komanso mphamvu yabwino kwambiri ya kutentha, HastelLoyx yakhala ikugwiritsidwa ntchito kwambiri m'malo osiyanasiyana otentha.
Minda yodziwika bwino yogwiritsira ntchito:
Ma turbines opangira mafakitale ndi ndege (zipinda zoyaka moto, zowongolera, zipewa zamapangidwe)
Zida za ng'anjo ya mafakitale, zodzigudubuza zothandizira, ma grates, riboni ndi machubu a radiator
Machubu ozungulira mu ng'anjo za petrochemical
Mpweya wotentha kwambiri umaziziritsa nyukiliya

            

Sekonic metal Technology Co., Ltd. mbale yoperekera mbale, mizere, chitsulo chozungulira, chitoliro, waya, forgings, ingot, flange, tee, chigongono, mafotokozedwe athunthu ndi mitundu
zakuthupi
Standard: Aloyi zitsulo F5 ndi 410; Chitsulo chosapanga dzimbiri 304, 304L, 316, 316L, 321 ndi 347.
Non-standard: mkulu faifi tambala aloyi (inconel 718, inconel 625, inconel 825, inconel 925, aloyi 20, GH3030, nimoni 80A), kutentha aloyi zitsulo (haines 25,25, haines 188, etc.)
Chitsimikizo chamtengo wapatali, mtengo wotsika mtengo, nthawi yochepa yobweretsera, perekani chitsimikizo choyambirira cha fakitale, ngati mukufuna kulandiridwa kuti muyimbire foni yam'manja / whatsapp: 0086-15921454807


  • Zam'mbuyo:
  • Ena:

  • Lembani uthenga wanu apa ndikutumiza kwa ife